LEADER |
01001naa a2200277 i 4500 |
001 |
NSK01000949954 |
003 |
HR-ZaNSK |
005 |
20161229114214.0 |
007 |
ta |
008 |
161129s2014 ci | |0|| ||eng |
035 |
|
|
|a (HR-ZaNSK)000949954
|
040 |
|
|
|a HR-ZaNSK
|b hrv
|c HR-ZaNSK
|e ppiak
|
042 |
|
|
|a croatica
|
044 |
|
|
|a ci
|c hr
|
080 |
1 |
|
|a 669
|2 MRF 2011.
|
100 |
1 |
|
|a Tawengi, A. S.
|
245 |
1 |
0 |
|a Cold weld cracking susceptibility of high strength low alloyed (HSLA) steel NIONIKRAL 70 /
|c A. S. Tawengi, A. [Aleksandar] Sedmak, V. [Vencislav] Grabulov.
|
300 |
|
|
|b Ilustr.
|
504 |
|
|
|a Bibliografija: 10 jed.
|
653 |
|
0 |
|a Legirani čelik
|a Hladne pukotine
|a Tvrdoća
|
700 |
1 |
|
|a Sedmak, Aleksandar
|
700 |
1 |
|
|a Grabulov, Vencislav
|
773 |
0 |
|
|t Metalurgija (Sisak)
|x 0543-5846
|g 53 (2014), 4 ; str. 624-626
|w nsk.(HR-ZaNSK)000013552
|
981 |
|
|
|b B09/14
|
998 |
|
|
|a lblo1611
|a rped1612
|
856 |
4 |
2 |
|u http://hrcak.srce.hr/index.php?show=clanak&id_clanak_jezik=180686
|y Elektronička verzija članka
|