LEADER |
01124naa a2200301 i 4500 |
001 |
NSK01000953826 |
003 |
HR-ZaNSK |
005 |
20170131111031.0 |
007 |
ta |
008 |
170120s2014 ci | |0|| ||eng |
035 |
|
|
|a (HR-ZaNSK)000953826
|
040 |
|
|
|a HR-ZaNSK
|b hrv
|c HR-ZaNSK
|e ppiak
|
041 |
0 |
|
|a eng
|b hrv
|
042 |
|
|
|a croatica
|
044 |
|
|
|a ci
|c hr
|
080 |
1 |
|
|a 67/68
|2 MRF 2011.
|
100 |
1 |
|
|a Yoshihara, Hiroshi
|
245 |
1 |
0 |
|a Mode I critical stress intensity factor of medium-density fiberboard obtained by single-edge-notched bending test /
|c Hiroshi Yoshihara, Hikaru Mizuno.
|
246 |
1 |
1 |
|a Faktor kritičnog intenziteta naprezanja (I. mod) MDF ploča dobiven testom savijanja
|
300 |
|
|
|b Ilustr.
|
504 |
|
|
|a Bibliografija: 14 jed.
|
504 |
|
|
|a Sažetak
|
653 |
|
0 |
|a Drvena građa
|a Ploče vlaknatice
|a MDF ploče
|a Naprezanje
|
700 |
1 |
|
|a Mizuno, Hikaru
|
773 |
0 |
|
|t Drvna industrija
|x 0012-6772
|g 65 (2014), 2 ; str. 99-104
|w nsk.(HR-ZaNSK)000015240
|
981 |
|
|
|b B10/14
|
998 |
|
|
|a mamo1701
|a dald1701
|
856 |
4 |
2 |
|u http://hrcak.srce.hr/index.php?show=clanak&id_clanak_jezik=181941
|y Elektronička verzija članka
|