Friction stir welding of new electronic packaging materials SiCp/Al composite with T-joint

Using friction stir welding, the electronic container box and lid made from aluminium matrix composites with reinforcement of SiC particle (15 vol% SiCp/Al-MMCs) was welded successfully with T-joint. The temperature distribution of box during the process, mechanical property and microstructure of th...

Full description

Permalink: http://skupni.nsk.hr/Record/nsk.NSK01001046193/Details
Matična publikacija: Engineering review (Online)
38 (2018), 3 ; str. 352-359
Glavni autori: Gao, Zeng (Author), Feng, Jianguang, Yang, Huanyu, Pakkanen, Jukka, Niu, Jitai
Vrsta građe: e-članak
Jezik: eng
Predmet:
Online pristup: https://doi.org/10.30765/er.38.3.12
Hrčak
LEADER 02319naa a22003854i 4500
001 NSK01001046193
003 HR-ZaNSK
005 20191120130530.0
006 m d
007 cr||||||||||||
008 191108s2018 ci a |o |0|| ||eng
024 7 |2 doi  |a 10.30765/er.38.3.12 
035 |a (HR-ZaNSK)001046193 
040 |a HR-ZaNSK  |b hrv  |c HR-ZaNSK  |e ppiak 
041 0 |a eng  |b eng 
042 |a croatica 
044 |a ci  |c hr 
080 1 |a 621  |2 2011 
100 1 |a Gao, Zeng  |4 aut 
245 1 0 |a Friction stir welding of new electronic packaging materials SiCp/Al composite with T-joint  |h [Elektronička građa] /  |c Zeng Gao, Jianguang Feng, Huanyu Yang, Jukka Pakkanen, Jitai Niu. 
300 |b Ilustr. 
504 |a Bibliografija: 16 jed. 
504 |a Abstract. 
520 |a Using friction stir welding, the electronic container box and lid made from aluminium matrix composites with reinforcement of SiC particle (15 vol% SiCp/Al-MMCs) was welded successfully with T-joint. The temperature distribution of box during the process, mechanical property and microstructure of the joint as well as gas tightness of welded box was investigated. The experimental results indicated that the satisfactory T-joint can be obtained under appropriate friction stir welding parameters. During the welding process, the bottom center, which was used to place the electronic component, reached a quite lower temperature of 100°C. That can ensure safety of components in the box. After the welding process, the microstructure in stir zone was better than in base material due to the refining and homogeneous distribution of the SiC particles. The experimental results showed that the electronic container box after friction stir welding had gas tightness. The He-leakage rate was under 10-8 Pa•m3/s. 
653 0 |a Kompozitni materijali  |a Metalni kompoziti  |a Zavarivanje 
700 1 |a Feng, Jianguang  |4 aut  |9 HR-ZaNSK 
700 1 |a Yang, Huanyu  |4 aut  |9 HR-ZaNSK 
700 1 |a Pakkanen, Jukka  |4 aut  |9 HR-ZaNSK 
700 1 |a Niu, Jitai  |4 aut 
773 0 |t Engineering review (Online)  |x 1849-0433  |g 38 (2018), 3 ; str. 352-359  |w nsk.(HR-ZaNSK)000848891 
981 |b Be2018  |b B02/18 
998 |b tino1911 
856 4 0 |u https://doi.org/10.30765/er.38.3.12 
856 4 1 |y Digitalna.nsk.hr 
856 4 0 |u https://hrcak.srce.hr/201158  |y Hrčak