Research on the grinding performance of high pressure sintering SiCp/Al matrix composites

The two-dimensional vertical grinding test equipment was used to grind SiCp/Al composites which were prepared by high pressure sintering method. The SEM observation of grinding morphology showed that grinding damage can be prevented by SiC particles reinforcement, 60% volume fraction of SiC particle...

Full description

Permalink: http://skupni.nsk.hr/Record/nsk.NSK01001046212/Details
Matična publikacija: Engineering review (Online)
38 (2018), 2 ; str. 175-181
Glavni autori: Chen, Zhiru (Author), Changyun, Li, Xu, Lei, metalurg, Mi, Guofa, Hu, Yukun
Vrsta građe: e-članak
Jezik: eng
Predmet:
Online pristup: https://doi.org/10.30765/er.38.2.5
Hrčak
LEADER 02010naa a22003854i 4500
001 NSK01001046212
003 HR-ZaNSK
005 20191120114501.0
006 m d
007 cr||||||||||||
008 191108s2018 ci a |o |0|| ||eng
024 7 |2 doi  |a 10.30765/er.38.2.5 
035 |a (HR-ZaNSK)001046212 
040 |a HR-ZaNSK  |b hrv  |c HR-ZaNSK  |e ppiak 
041 0 |a eng  |b eng 
042 |a croatica 
044 |a ci  |c hr 
080 1 |a 621  |2 2011 
100 1 |a Chen, Zhiru  |4 aut 
245 1 0 |a Research on the grinding performance of high pressure sintering SiCp/Al matrix composites  |h [Elektronička građa] /  |c Zhiru Chen, Changyun Li, Lei Xu, Guofa Mi, Yukun Hu. 
300 |b Ilustr. 
504 |a Bibliografija: 22 jed. 
504 |a Abstract. 
520 |a The two-dimensional vertical grinding test equipment was used to grind SiCp/Al composites which were prepared by high pressure sintering method. The SEM observation of grinding morphology showed that grinding damage can be prevented by SiC particles reinforcement, 60% volume fraction of SiC particles of SiCp/Al composite can hinder grinding depth and grinding performance was improved with the sintering pressure and temperature increasing. In addition, some scratches and exfoliated pits of SiC particles were observed on the surface of 60% volume SiCp/Al composite as the increase of grinding grain, while the depth of these scratches was shallower, there was no large area exfoliated pits of SiC reinforcements. 
653 0 |a Kompozitni materijali  |a Metalni kompoziti  |a Silikatni materijali  |a Sinteriranje 
700 1 |a Changyun, Li  |4 aut 
700 1 |a Xu, Lei,  |c metalurg  |4 aut 
700 1 |a Mi, Guofa  |4 aut 
700 1 |a Hu, Yukun  |4 aut  |9 HR-ZaNSK 
773 0 |t Engineering review (Online)  |x 1849-0433  |g 38 (2018), 2 ; str. 175-181  |w nsk.(HR-ZaNSK)000848891 
981 |b Be2018  |b B02/18 
998 |b tino1911 
856 4 0 |u https://doi.org/10.30765/er.38.2.5 
856 4 1 |y Digitalna.nsk.hr 
856 4 0 |u https://hrcak.srce.hr/196254  |y Hrčak