Some characteristic physical properties of nickel oxide powder
Nickel oxide powder was prepared by firing spec pure NiCO3 in air for 6 hours at different firing temperatures ranged from 800°C to 1200 °C. The crystal structure of all samples is a cubic structural as obtained from XRD study. The diffuse reflectance of different samples of NiO was measured at room...